Thursday, May 14, 2015

[MW:23280] combine 2 procedures in AWS D1.1

Dear Experts,

I have GTAW and SMAW procedure qualified seperately as per AWS D1.1.  Can we  prepare one WPS with these 2 qualified procedure as root run GTAW and subsequent run SMAW.

GTAW qualified in  8 mm thk  S 275 JR and SMAW qualified in 25 mm thk S 275 JR as per AWS D1.1

Thanks in advance.
Manoj

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACgUO5kmghaqAQH7U7bw48W6r8ApvJGzvHzd2YpZAPn4znPS5A%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...