Wednesday, May 13, 2015

[MW:23275] Hey Dear Experts, what is the different between welding SS316 and 317?

Hey, it is my first time here, as post may I have your comment on welding SS317 reactor?
Any specified attention should be paid during welding supervision?
Thanks a lot.
 