Hi Vishwas,
 
PWHT cycle ,T& T, rate of heating /rate of cooling should be as per the piping design codes, e.g B-31.1 or 31.3 or others as  specified in the drawings or specifications.
 
AWS D-10.10 should be followed also as a guiding document for setting up equipments, e.g, heating pads, thermocouples,.....to facilitate the PWHT. In fact you need to to look at D-10.10 for detailed  guidelines, assuming these pipes would not be heat treated in in furnace.
 
Thanks
 
 
Pradip Goswami, P.Eng,IWE
Welding & Metallurgical Engineer/Specialist
Ontario, Canada
 




On Tuesday, May 26, 2015 at 10:19:30 AM UTC+5:30, Vishwas Keskar Welding Manager Pune India wrote:
For long piping(Carbon steel, alloy steel), butt welding of large diameter(219mm OD TO 606mm OD, THK - 18.26mm to 42 mm )pipes is carried out. 
For PWHT of these butt welds, what are the parameters shall be considered for effective PWHT?

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4a044795-1847-4745-a576-efbc881ee423%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...