[MW:23048] P1 to P43 Dissimilar Joint PWHT Requirements

If you have PQR of ENicrMo3 weld built up on P1 material to P43, then it is the best solution for this joint.

If with PWHT with impact test vessel, then you should follow same procedure for this production joint.

--