Thursday, May 21, 2015

[MW:23002] WPS with groove welding will also qualify Fillet welding.

Dear Experts, 

Can any one suggest if Groove welding WPS will also allow welding with fillet. please guide with reference standard clause.

--
Thanks and Regards, ?

Mohammed Ghani,

CSWIP 3.1 / BGAS L-2 / ISO 9001:2008 QMS LA.

Mechanical Inspector,
BUREAU VERITAS.


ü
 Please consider the environment before printing this email.

 "Be the change you wish to see in the world"

---Mahatma Gandhi---

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAG7AWVjjPwZ%2BkvBBQ-mQ1p1XV0tjtSv4jh8vqu-icwtVMpD%2B7g%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...