Please refer below,

QW-404.35 A change in the flux/wire classification or a change in either the electrode or flux trade name when not classified in an SFA specification. Requalification is not required when a wire/flux combination conforms to an SFA specification and a change is made from one diffusible hydrogen level to another (i.e., a change from F7A2‐EA1‐A1H4 to F7A2‐EA1‐A1H16). This variable does not apply when the weld metal is exempt from impact testing by other Sections. This exemption does not apply to hard facing and corrosion‐resistant overlays.

-- 
With Best Regards, 
Vijay.A.Malusare
Engineer

On Thu, Apr 16, 2015 at 2:17 PM, 'raouf salhi' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Dear Aly ;

There is no problem to change ( we have the same classification and specification according ASME sect. IX).

Regards
 
SALHI Raouf
QA/QC Engineer

Tel: Morocco +212628979891
      Tunisia +21621458258



Le Mercredi 15 avril 2015 15h18, Mhaskar Aly <mhaskar.aly@gmail.com> a Ʃcrit :


Dear All,
We have PQR of following details:
 
Process SAW with Filler Wire EM12K (ESAB) with Flux F7A8 (ESAB OK 10.62 Flux)
 
Question:
1.       Can we use Filler Wire EM12K (Bohler) with Flux F7A8 (ESAB OK 10.62 Flux)
2.       Can we use Filler Wire EM12K (Bohler) with Flux F7A8 (Bohler Flux)
 
Kindly advise as per ASME Sec IX…with reference.
 
Thanks in advance
 
 
Ali Mhaskar,
QA/QC Manager
Velath Engineering International FZC; Hamriyah FreeZone Sharjah, UAE; * P.O Box 6268 – Sharjah UAE.
(Phone: 00971-6-526 9269, 526 9185, 526 9119 Ext-212 ƈMobile no.: 00971-55 265 3598 ÊFax no. 00971-6-526 9393  üwww.velath.com
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOenW4htWh-B5O0xAn_yPAbYpWWRcX6NWmDT5tmmziG3jgPAxQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/116381582.4884065.1429174055534.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.





--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADAKtxmXA5bqSTCePpba2WJteYgYkiOn6ukemTPge0r0tSCWCw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...