Skip to main content

Re: [MW:23070] RE: 23061] RT Report clarification / advise required

Dear Sir,

You are correct and just for curiosity what is your vendors interpretation for that paragraph.

Regards,

Hareesh K V

On Apr 9, 2015 8:28 AM, "Lakshman" <lakshmankumar4@gmail.com> wrote:
Hi friend, you are correct, but let us understand why client is not accepting and what is his views?
We should know theirs interpretation also prior to confirm...😊

Lakshman kumar.B
Project manager.
9440031459

From: Mohammed Ismail
Sent: ‎09-‎04-‎2015 08:00
To: materials-welding@googlegroups.com
Subject: [MW:23061] RT Report clarification / advise required

Dear Experts,

 

I am pleased to draw your attention and please provide your valuable input / advice / comment / clarification regarding my interpretation as below.

 

The following is the requirement as referring to the attached 6600028289 (OOK) schedule Q_quality requirements attachment 1 clause 2.2.1.

 
Quote starts 


" When performing, reviewing or ensuring Nondestructive Testing in VT, MT, PT, RT or UT, he shall be certified in the specific method(s). When performing, reviewing or ensuring Radiographic Testing Film Interpretation (), Inspector shall be certified in ASNT Level II."


Quote Ends

 

My interpretation is RT report shall be reviewed or ensured by the inspector with ASNT Level II certified in RTFI.

And after reviewing or ensuring the reports as per the requirements that report shall endorsed (singed) by that inspector who is qualified in RTFI .


But the vendor is dis agreeing with the my statement.

 

Please advise me. 


Thanks and best regards,

Mohammed Ismail,

Mechanical Inspector,

vendor inspection department,

Velosi.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAF2Z%3DtU1K6RTNjHkkjN1ibYNxK3VNSufzza5j4BgLah%2Bx%2BYAJg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5525e7c3.e26e440a.3a8a.2d95%40mx.google.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM3LgAVxyZJcSoB1Q%2BwyGKz7c19hf8CS872ruAy8pXCr5vSmzw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...