In general UT for clad plates is done based SA 578.
SA 578 allows disbanding as per Level A,B & C, etc...

On Thu, Dec 4, 2014 at 6:20 AM, MATERIAL <khare1963@gmail.com> wrote:
Hi,
Our company spec.(BP) permits acceptance of disbonding upto 1000 mm sq.
Yes the clad is corrosion resistance and service is high pressure hydrocarbon.
On Wednesday, 3 December 2014 13:21:37 UTC+8, sina wrote:
Dear friend
May I ask which code permits dis-bonding in clad? As I guess your clad is corrosion resistance.



On Tue, Dec 2, 2014 at 9:38 AM, MATERIAL <khar...@gmail.com> wrote:
Dear Friends,
 
Noting that every clad mother plate will have some acceptable disbonding,however,spinning/forming of various dish ends can increase it to unacceptable limits.
I would like to ask our gurus about what are the causes of disbonding happening during dish spinning process and how to avoid the same.
 
 
Regards.
 
Ashwani Kumar Khare

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
M. Shokri Arfaei
ISA-ISTS - Metallurgy Lab. Manager
ASNT NDT Level III
International Welding Engineer





--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35544] WELDING OF SS 310 MATERIAL CRACK ISUUE..

We are doing a welding of SS 310 Material Plate with ER310 Grade welding electrode... But its contineous cracking.... at welding line,,,,......