Re: [MW:22476] Selection of IQIs

Please bear in mind ASME V & API 1104 are referencing codes and not code of construction.
The code of construction are generally ASME Sec VIII Div. 1/2 or B 31.1, 31.3 for Sec V and B31.4, 31.8 or API standards for API 1104.
ASME & API follow different philosophy with respective to their std/ code.  

On Wed, Dec 3, 2014 at 2:54 PM, AHMAD&MOHAMAD REDA <amreda2006@gmail.com> wrote:

Dear experts

 

There is a major difference between the selection of IQI for DWSI according to ASME V article 2 & API 1104 

 

ASME sec v T-276.2    (2013) -1

Based on single wall thickness + reinforcement

 

2- API 1104 (11.1.5)         (2013)

Based on twice wall thickness + reinforcement internal &external

 

(copy attached for the two statements)

 

IT MEANS THAT

The same weld and the same technique but the essential wire diameter differs!!!!!!!!

Please advice and if there is an ASME Inspector to consult the ASME to make this relaxation because it makes a big difference. 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35597] INCONEL 825

Dear all  INCONEL 825 matching filler   ER NI FECR-1 its correct please guide me Regarding  Elavarasan -- https://materials-weldin...