Dear friend
This issue is related to your work scope.
For example, you personnel should measure dimensions of a bolt (e.g the length) 200mm which is permitted in the procedure to be 195 to 205mm. The procedure also requires that measurements done with accuracy in tenth of millimeters (0.1mm). So :
1- They should select a measuring devices that cover in the minimum the range of use (195-205mm).
2- They should select a measuring devices that could show the measurements in tenth of millimeters (0.1mm).
3 - the calibration agency should report you the accuracy of the device in tenth of millimeters. (If they report the accuracy in millimeters, this is under qualified and if the report in hundredths of millimeters it is overqualified.
I hope this could make your answer.
Regards
On Fri, Dec 5, 2014 at 6:24 PM, Saravanan Sornam <saravanshyla@gmail.com> wrote:
Mr.Vairamuthu, i know that the master calibration shall be traceable to international standard and that is ok but my query is,
How the QC manager set the accuracy level, for gages, vernier calipers , pressure gages, when he review the calib cert. .
Give me some samples.
Regards
Sarav.On Dec 5, 2014 11:51 AM, "Vairamuthu Ramar" <vairamuthu78@hotmail.com> wrote:----
Please refer the point no.5 in the certificate attached by you which describes - Traceability of the Master instrument details.
This master instrument only used for calibration of your clampmeter.
If you see the master instrument calibration certificate which might be available with your calibration agency you can come to know that this (master instrument) is calibratied by Internationally Recognised Authorities/Approved Agenicies.
So usually all equipments/instrument are calibrated by these Master Instruments which are traceble to Internationally Approved Calibration Laboratory Certificate.
Regards,
R Vairamuthu
Date: Thu, 4 Dec 2014 16:19:21 +0900
Subject: [MW:22452] Calibration Accuracy Info In Cert
From: saravanshyla@gmail.com
To: materials-welding@googlegroups.comDear Experts ,I have attached a sample Calibration Cert for AC DC Clamp Meter.My query is, when QC team receive this calibration cert which is calibrated by outside testing lab,how the QC confirm the accuracy or confidence level and on what basis, when they approve this certificate for usage.I would like to know for Pressure Gages, Vernier Calipers, Micrometer, QC DC Clamp Meter, digital temperature Gun, etcRegards,Saravanan
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
M. Shokri Arfaei
ISA-ISTS - Metallurgy Lab. Manager
ASNT NDT Level III
International Welding Engineer
Tel.: +98 21 66282127
Fax: +98 21 66282779
Mob.:+98 912 1394023
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
No comments:
Post a Comment