Saturday, March 1, 2014

Re: [MW:20208] NDT Acceptance criteria for IBR welds

Dear sir,
I do not see in either regualations how a weld with some indications are accepted or rejected. Both these regulations refer to general requirements.
 
With Best Regards,
Shashank C Vagal


On Saturday, 1 March 2014 4:02 PM, Shashank Vagal <nach_sam@yahoo.com> wrote:
Thanks. I will check.

 
With Best Regards,
Shashank C Vagal


On Saturday, 1 March 2014 2:19 PM, CHINTUKUMAR GANDHI <cgandhi1975@yahoo.com> wrote:
Dear Sir,

Regualtion NO. 265 & 560 of IBR 1950 Ed. 2007.

Thanks & regards,


C. R. GANDHI


From: Shashank Vagal <nach_sam@yahoo.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>; Nachi <nachi.vagal@gmail.com>
Sent: Friday, February 28, 2014 11:17 PM
Subject: [MW:20195] NDT Acceptance criteria for IBR welds

Gents,
Where can we find details of NDT Acceptance criteria for IBR job related welds? It is not found in IBR 1950 book. Or may be I missed it.
 
With Best Regards,
Shashank C Vagal (Quality Adviser)

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.




No comments:

[MW:35346] Cast-iron welding

Any advice for cast iron welding Sent from Yahoo Mail for iPhone