My friend ,Sch 40 =STD (standard wall thickness) and Sch xs = Sch 80(extra strong wall thickness) and Sch xxs= Sch 160 ( extra extra strong wall thickness)

Regards,
Ricardo Erasmus ( Welding Superintendent) Kentz


On Sat, Oct 12, 2013 at 3:23 PM, James Abraham <jamesmundokulthu@yahoo.com> wrote:
Dear Members
I have the following doubts to clear in the fabrication of large bore CS  pipe
As per our contract all the large bore pipes are Sch 40 but they provide the material and as per the design all the pipes are Sch  XS
1, What is thickness difference between Sch 40 & XS and how  I can prove this one according to the international standard
2. I have any wright to claim for extra cost because of the thickness difference

Please give your valuable advice

Thank You 

BEST REGARDS

JAMES ABRAHAM|Email - jamesmundokulthu@yahoo.com

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...