[MW:18971] Re: Welding of CuNi 70/30 to SA106

Thanks to all 
I am going to weld with ER Ni-1 for buttering and remaining by ER NiCu-7 
and late you know the test result. 

On Wednesday, October 9, 2013 9:08:51 AM UTC+5:30, prabhu wrote:
Dear All,
Can anyone tell me which filler should be used for welding CuNi 70/30 to SA106. by using GTAW process.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...