---------- Original message ----------
From:"Prakash"< prakashnorway@in.com >
Date: 6 Sep 13 17:27:24
Subject: Urgent Help Required Folks........As per Norsok can we accept 5mm pore in material that are centrifugal casted ?
To: materials-welding@googlegroups.com
Hi Experts,I am working on Ferritic/Austenitic Stainless Steel, Type 25Cr duplex centrifugal casted product.(For cylinder part for SUBSEA).
As per Norsok MDS D56 details are below :
PRODUCT STANDARD GRADE SUPPL. REQ.
Castings ASTM A 995 5A (UNS J93404) 6A (UNS J93380) - S5, S6, S20
NON DESTRUCTIVE
TESTING
Liquid penetrant testing: Supplementary requirement S6 shall apply to all surfaces
(including internal surfaces) of all castings. The testing shall be carried out after final
machining and pickling. The acceptance criteria shall be ASME VIII, Div. 1, Appendix 7.
Radiographic testing: Supplementary requirement S5 shall apply to:
- Critical areas as per ANSI B16.34 of the pilot cast of each pattern
- All butt weld ends of each casting
- Class 1500 psi and above; all critical areas to ANSI B16.34 of each casting.
The acceptance criteria shall be to ASME VIII, Div. 1 Appendix 7.
NDT operator qualification shall be approved by a 3rd party organization recognized by an EC member state.
Experts, If possible please respond on above query ASAP.
Regards,
Prakash
+47-91275122
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
No comments:
Post a Comment