Wednesday, July 31, 2013

Re: [MW:18320] Prequalified WPS as per AWS D1.1




  Dear Dinesh

Your answer is partially correct make a note Pre- Qualified WPS  covers Partial Penetration (P.P) & Complete Penetration ( C.P.)  Joints  Hence Pre Qualified WPS  are applicable to STATIC LOADING
 AS WELL AS DYNAMIC LOADING. Pre Qualified WPS is a proposed WPS & Needs Actual Testing before Procedure Qualification Test.

 Regards

Dr. Rajan Gupte- Welding Expert ( US & UK )
Chartered Surveyor    
 



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...