Hi 

It appears that there is some mix up of welding consumables like ER316L.
Please check the welding consumables issue slip and find out whether there was any mixup.

Rectification is to remove the defective areas by grinding and reweld as per WPS.

Regards

Prem Nautiyal



From: Harikrishnan N S <hari.qaqc@gmail.com>
To: materials-welding@googlegroups.com
Sent: Tuesday, July 30, 2013 9:17 AM
Subject: [MW:18292] High Ferrite No.

Dear Experts

Recently I came across an issue of High Ferrite no. in the weld metal.

Parent Metal : A 304L
Weld Metal : 308L
Welding Process : GTAW

The affected area is only a quarter portion (3'o clock to 6'o clock position) of the 30" pipe where ferrite no has been observed as over 21 FN. and PMI has shown 1.57% of Mo. 

Please give your valuable comments and rectification measures for this. Refer the attached photos for clarity.

Thanks and Regards
Harikrishnan
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 


No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...