Re: [MW:18282] Material Thickness Inspection

Yes acceptable, UG-16 (c) only for min required thickness 

Ur case not issue bcz received thickness more than required thickness 

Regards, 

Vidhyapathi 

On 27 Jul, 2013, at 7:42 PM, AAMIR SADDIQ <aamirtec301@gmail.com> wrote:

Dear Expert,

                    Please Cleared my doubt,

ASME SECTION VIII UG-16. (c) Mill Undertolerance. Plate material shall be ordered not thinner than the design thickness. Vessels made of

plate furnished with an undertolerance of not more than

the smaller value of 0.01 in. (0.25 mm) or 6% of the

ordered thickness may be used at the full design pressure

for the thickness ordered.

 

Ok I understand not less than the above Tolerance.

 

 If the specification to which the plate is ordered allows a greater undertolerance, the ordered thickness of the materials shall be sufficiently greater than

the design thickness so that the thickness of the material

14 furnished is not more than the smaller of 0.01 in. (0.25 mm)

or 6% under the design thickness.

I don't understand not more than the smaller of 0.01 in. (0.25 mm)

or 6% under the design thickness. Actually we required a plate thickness 121mm but we received 122.8mm thickness. this excess Thickness acceptable. 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...