Friday, July 19, 2013

[MW:18222] [18149] WQT According to AWS D1.8

This term is used in US standards for certain welded joints in seismic (earthquake) applications. Under the AWS D1.8 Structural Welding Code – Seismic Supplement, the welder who welds the bottom flange of a beam to a column flange, through a weld access hole, is to take a specific weld test using a mock-up of the joint to ensure he/she has the proper techniques to weld the CJP groove (butt) weld through the weld access hole. The AISC Seismic Provisions (AISC 341-10) and AISC 358 seismic connections standard provide information as to what welds are deemed “demand critical”.

 

Bob Shaw

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Tarek Yehia
Sent: Thursday, July 11, 2013 11:58 AM
To: materials-welding@googlegroups.com
Subject: [MW:18149] WQT According to AWS D1.8

 

Dear Experts,

Can any one tell me more about the above subject? Also is any one have it softcopy?

Our client is requiring welders to be qualified for some "Demand Critical Weld".

If any one performed such WQT...please send me copy of this qualification.

Thanks,

Regards,
Tarek Yehia

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...