Dear Sir,

 

When you have a project where it is required to have WPS regarding EN-ISO 15609 (BS-EN 288 is withdrawn) you should have a PQR qualified according to EN-ISO 15614-1 for Steel and Nikkel base alloys.

When your project specification still mentions BS-EN 288 you should have a PQR qualified according to BS-EN 288-3.

It is not allowed to use ASME IX PQR’s for drawing up EN-ISO WPS documentation.

 

Met vriendelijke groeten / Best Regards,

 

Herman Pieper

QA-QC Inspector / IWI-C / IWT / Materials expert

 

Job van der Havestraat 6

8384 DB, Wilhelminaoord

Tel: 06-51691215

 

Van: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] Namens Shanmuganathan Subbiah
Verzonden: zondag 11 november 2012 6:55
Aan: materials-welding@googlegroups.com
Onderwerp: [MW:15902] is possible qualifed asme sec ix wps can change to bs 288-3 format

 

Dear experts,

 

i have one PQR  which one was qualified as per asme sec ix, now i want to prepare wps as bs288 format by use of qulified PQR.

 

is it possible?
--

Regards

SHANMUGANATHAN SUBBIAH

--
To post to this group, send email to
materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...