Re: [MW:15907] is possible qualifed asme sec ix wps can change to bs 288-3 format

hi Shanmugam,

both codes are entirely different testing and qualification requirements, different essential variables, so you cannot make it.

For BS EN 288, you qualify it separately.

Cheers,
Saravanan Sornam,
Anseong, Korea
 

On Sun, Nov 11, 2012 at 2:55 PM, Shanmuganathan Subbiah <shanmuganathan.subbiah@gmail.com> wrote:
Dear experts,
 
i have one PQR  which one was qualified as per asme sec ix, now i want to prepare wps as bs288 format by use of qulified PQR.
 
is it possible?
--

Regards

SHANMUGANATHAN SUBBIAH

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...