Sunday, November 11, 2012

Re: [MW:15911] Backing strip/ring material acceptance.

Refer ASME B 31.3 - 2010 , Clause 311.2.4 and 328.3.2

 ವಂದನೆಗಳೊಂದಿಗೆ / Best regards,

Nandesh Kumar A
ABS Group Inc.
Abu Dhabi, UAE

P.S. : Please don't print this e-mail unless you really need to.


From: Biplab Pal <biplab.mech@googlemail.com>
To: materials-welding <materials-welding@googlegroups.com>; JALADHAR JENA <jdjena2006@yahoo.co.in>; Pinaki Boxi <boxi.pinaki@gmail.com>; chandan.majumdar <chandan.majumdar@sgs.com>; daval shaikh <davalshaikh@gmail.com>
Sent: Sunday, 11 November 2012 8:52 AM
Subject: [MW:15904] Backing strip/ring material acceptance.

Dear Experts,
 
Our contractor is going to use the backing strip(permanent) for pipe welding.
As per ASME B 31.3 the material will be acceptable if Sulpher content remains less than 0.05%.
Can anybody give a light on backing strip/ring material acceptance for piping. Please provide me the references.

--
Thanks & Regards
Biplab Pal
Welding Inspector
E-mail:   biplab.mech@gmail.com
 
Information in this email and any attachments is confidential and intended solely for the use of the individual(s) to whom it is addressed or otherwise directed. Please note that any views or opinions presented in this email are solely those of the author and do not necessarily represent those of the Company. Finally, the recipient should check this email and any attachments for the presence of viruses. Myself accepts no liability for any damage caused by any virus transmitted by this email.
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 


No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...