Re: [MW:15019] Which Electrode/Filler wire we should use for 12Cr1MoV ?

 
It is a Chinese Material indeed.
you may choose R317 for SMAW and R31 For GTAW  to weld 12Cr1MoV.


On Fri, Aug 3, 2012 at 6:40 AM, Roy Liu <standardliu@hotmail.com> wrote:
Hi,
 
It is a Chinese Material indeed.
you may choose B2V (8018-B2V) to weld 12Cr1MoV.
China Mainland use only........
 
Roy
Bohler Welding
 
 
Sent: Tuesday, July 31, 2012 12:05 PM
Subject: [MW:14993] Which Electrode/Filler wire we should use for 12Cr1MoV ?
 
Dear Experts,
 
In Thermal Power we have material of Strape plate is 15CrMo & we are using E8018B3,
 
Now New material 12Cr1MoV is coming for structure & piping work. Can we use ER 90SB3 + E9018 B3 ?which electrode & filler wire we should use as per standard.
 
If Not kindly suggest me Which Electore & filler wire should we use, as per the standards.
 
Waiting for Reply.
 
Regards.
 
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Santosh B Patil
Welding Engineer
SEPCOIII
Mob No 9725501785


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35374] Material Certification 3.1 / 3.2/2.2--EIL India

Dear Perumal, I answer the same but got one more question where it is written that TPI witness is mandatory? -- https://materials-...