Re: [MW:15017] change in electrode class

Dear Mr, John,

I agree, i was incorrect about welder qualification.
actually i was confused with f-6..
thanks
yes welder can weld.


On Thu, Aug 2, 2012 at 6:18 PM, John Henning <jhenning@deltak.com> wrote:
Mr Biplab Pal,

Your last statement regarding welder qualification is incorrect.  Please
look at QW-433 "Alternate F-Numbers for Welder Performance
Qualification", which specifically addresses SMAW.

Qualification with F4 will additionally qualify the weldor for F3, F2,
and F1.
Qualification with F3 will additionally qualify the weldor for F2, and
F1
Qualification with F2 will additionally qualify the weldor for F1

John A. Henning
Welding & Materials

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of Biplab Pal
Sent: Wednesday, August 01, 2012 9:41 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:15005] change in electrode class

Dear Mr. Pankaj Kolhe,

If you are using ASME SEC IX 2010 then you can not use.
For SMAW Process F number is Essential Variable for welding procedure
qualification and F Number of E6013 is 2 and F number of E7018 is 4.

And for welder qualification F number also essential variable. So you
can not use different F number.

Reference QW 432, WQ 253, QW 353



On 8/1/12, pankaj.kolhe@wipro.com <pankaj.kolhe@wipro.com> wrote:
>
> Dear all,
> If the procedure is qualified on E7018 Electrode for SA 516 Gr 70 then

> can we use this WPS/PQR for welding IS2062 Gr B by E6013 electrode.
> Also for welder qualification can we use this WPS/PQR , Give code
> reference I think change in filler metal class is essential variable.
>
> With Regards,
> Pankaj Kolhe
> QC
> Wipro Water (Wipro Ltd)
> O- + 91 22 39302135
> M: +91 9323940892
>
> Wipro Limited.Serene Properties Private Limited,Special Economic
> Zone,3rd Floor,Building No. 7, Plot No.3,TTC Industrial Area,Thane
> Belapur Road,Opposite Airoli Rilway station.Airoli, Navi Mumbai-
> 400708,Maharashtra[cid:image002.gif@01CD6FD1.6B5D7F70]
>
> --
> To post to this group, send email to
> materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views

> and meant for educational purposes only, Users must take their own
> decisions w.r.t. applicable code/standard/contract documents.
>


--
Thanks & Regards
Biplab Pal
Mechanical Inspector (PMT)
YASREF Project

E-mail:   biplab.mech@gmail.com

Information in this email and any attachments is confidential and
intended solely for the use of the individual(s) to whom it is addressed
or otherwise directed. Please note that any views or opinions presented
in this email are solely those of the author and do not necessarily
represent those of the Company. Finally, the recipient should check this
email and any attachments for the presence of viruses. Myself accepts no
liability for any damage caused by any virus transmitted by this email.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.

______________________________________________________________________
The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.
______________________________________________________________________

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks & Regards
Biplab Pal
Mechanical Inspector (PMT)
YASREF Project

E-mail:   biplab.mech@gmail.com
 
Information in this email and any attachments is confidential and intended solely for the use of the individual(s) to whom it is addressed or otherwise directed. Please note that any views or opinions presented in this email are solely those of the author and do not necessarily represent those of the Company. Finally, the recipient should check this email and any attachments for the presence of viruses. Myself accepts no liability for any damage caused by any virus transmitted by this email.
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35374] Material Certification 3.1 / 3.2/2.2--EIL India

Dear Perumal, I answer the same but got one more question where it is written that TPI witness is mandatory? -- https://materials-...