Wednesday, August 1, 2012

Re: [MW:15002] Re:Crack in the shell with thickness of 82.6 mm After PWHT

Dear,
         there are few chances to crack this weld but make sure that the proper welding and after welding when we start the procedure of PWHT.if PWHT has done 86.7 c while its max cooling is 80 its not big issue normal cooling but the fault in ur welding or welding electrode .



Warm Regards:-
Liaqat Ikram
A.C Mechanic
+92-300-8626191

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...