Thursday, August 9, 2012

[MW:15045] Welding S355G8+N per EN 10225 :2001 standard.

Dear all,

Can anybody suggest the welding consumable used for welding subject materials.

It will be highly appreciable if some one provides preheat / post heat requirements if any.

We use these materials in offshore platforms- Jacket materials, thickness- 40mm.

Best regards

V.Rao.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...