Sunday, July 8, 2012

Re: [MW:14800] Connecting of ICCP electrodes to the oil pipe


Dear Mr. Manpreet Singh

Many thanks for your response…

Actually, I am working as a consultant engineer in crude oil tank construction project in the south of Iraq. They ask me to design ICCP system for tanks and underground pipe. Up to my information connecting of silicon iron electrodes to the tank body was known. The problem is how to connect electrode cable to the underground pipe, I think they used a special procedure to do that…..So, would you please help me with an information about the standard method or any other method….

Accept my profound regards…

 Dr. Eng. Alaa A. Atiyah
--- On Fri, 7/6/12, manpreet <manpreetsin88@rediffmail.com> wrote:


From: manpreet <manpreetsin88@rediffmail.com>
Subject: Re: [MW:14789] Connecting of ICCP electrodes to the oil pipe
To: materials-welding@googlegroups.com
Date: Friday, July 6, 2012, 11:20 PM

Hi,

Would you please describe the problem,

Regards,
Manpreet Singh


On Sat, 07 Jul 2012 11:24:22 +0530 wrote
>
>
>



Dear Experts

I have a problem during the connecting of Deepwell electrode cable to the oilpipe structure in one of the sites at the south of Iraq. The technical facilities there is limited. Would you please share your technical information with me.

Regards,
Dr. Eng. Alaa A. Atiyah





--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>


Follow Rediff Deal ho jaye! to get exciting offers in your city everyday.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...