Saturday, July 7, 2012

Re: [MW:14798] Filler Materail required for welding SS 321 to SA 516 gr-70

Hi!
Generaly E309L type filler is suitable for  welding of CS to SS321 material
Regards
 
Hegde p.B.

--- On Sat, 7/7/12, Ankit Patel <ankit.patel@orientalindia.net> wrote:

From: Ankit Patel <ankit.patel@orientalindia.net>
Subject: [MW:14790] Filler Materail required for welding SS 321 to SA 516 gr-70
To: materials-welding@googlegroups.com
Date: Saturday, 7 July, 2012, 4:50 PM

Dear Experts,

 

I want to weld SA 516 GR-70 plate to SA 182 TP 321.

 

Kindly suggest me the filler material grade used  for welding this material.

 

Thanks & Regards

Ankit Patel
Engineer Quality

 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...