Re: [MW:14795] SINGLE WPS WITH MULTIPLE PQR

Yes, you can use them. refer QW 200.4 (b) for the details.

sridhar


From: LALIT VADADORIYA <lalit.vadadoriya@gmail.com>
To: materials-welding@googlegroups.com
Sent: Thursday, 5 July 2012 4:16 PM
Subject: [MW:14770] SINGLE WPS WITH MULTIPLE PQR

DEAR EXPERTS
 
WPS FOR GTAW + SMAW PROCESS & SUPPORTING PQR (1) FOR GTAW 6" DIA PIPE HAVING 7.11MM THICK AND (2) PLATE HAVING 20 MM THICKNESS IS 2062 GR.B MATERIAL.
 
PIPE THICKNESS 1.5 -20 MM RESTRICTED
 
WPS QUALIFIED FOR GTAW-3MM AND SMAW 24.11MM THICKNESS,  CAN WE ACCEPTED THIS ONE OR NOT. 

--
Regards

Lalit Vadadoriya
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...