Saturday, July 7, 2012

Re: [MW:14794] Settlement of hydro test tanks - allowable limt

Dear Mr. Narsimharao,

650 is silent on the acceptable limits of settlement.  It does say, however that if settlement measurements are specified by the Purchaser, any differential settlement greater than 13 mm per 10 m (1/2 in. per 32 ft) of circumference or a uniform settlement over 50 mm (2 in.) 

On 7 July 2012 10:00, Narasimha Rao <narasimharao.kaja@gmail.com> wrote:
Hi All,
 
       I Would like to know how much settlement allowed during hydro test of floating roof tank.
       
        At my site, the tank foundations are placed on concrete pilings due to soft soil conditions.. Piling depth around 22 mtrs from ground level. Tank dia 40 Mtrs. Height 18 mtrs. Even after strong piling for every one meter distance ( pile to pile, pile dia 600mm).Around 150 piles layed below the tank foundation. During hydro test of tanks we observed at one side settlement around 100mm observed.
       
        What is the allowble settlement for tanks with piling and without piling foundations.In which API code mentioned.
 
       
 Regards.
 
K V Narasimha Rao
Sr. Principal Engineer
IRS - TPI
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--




Best Regard's,


Aron Luke G

אהרון  לוקאס

Mobile : +91 9000788879

            +91 9010788879

E-Mail : aronlukeg@gmail.com




SAVE PAPER - SAVE TREE - Please do not print this e-mail unless necessary.



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...