[MW:14846] Heating/cooling rate requirement for PWHT

Dear All,

As per ASME section NX-4623,Above 800°F(425) the rate of heating and cooling in any hourly interval shall not exceed 400°F(222)divided by the maximum thickness in inches of the material being heat treated,but shall not exceed 400°F(222)and need not to be less than 100°F(56)in an hourly interval.

 

Now the actual heating and cooling rate in our production we made is 50/hour which is less than 56/hour required above. Our custom insist that this is unacceptable and should be reheated. But my understanding is that the 56 is not a mandatory requirement and only the upper limitation is required. Do I understand this correctly? PLZ guide me! Appreciate it!

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...