Dear all,

I would like to know about the non purge wires for SS welding. Please share your experience for these wires. Are these economical wrt normal GTAW wires with Ar purging.

Thanks
Mukesh Kumar
Sent from BlackBerry® on Airtel

From: "Ankit Patel" <ankit.patel@orientalindia.net>
Sender: materials-welding@googlegroups.com
Date: Sat, 7 Jul 2012 16:50:22 +0530
To: <materials-welding@googlegroups.com>
ReplyTo: materials-welding@googlegroups.com
Subject: [MW:14790] Filler Materail required for welding SS 321 to SA 516 gr-70

Dear Experts,

 

I want to weld SA 516 GR-70 plate to SA 182 TP 321.

 

Kindly suggest me the filler material grade used  for welding this material.

 

Thanks & Regards

Ankit Patel