Tuesday, July 3, 2012

Fw: [MW:14750] Diameter Qualiffication Range for WPS per section IX

Hi Rafeeq,

Pl. refer to my earlier reply. WPS/PQR done on 8" dia. pipe qualifies all ranges of pipe diameters.
sridhar.

----- Forwarded Message -----
From: c sridhar <sridhar305@yahoo.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Tuesday, 3 July 2012 4:20 PM
Subject: Re: [MW:14747] Diameter Qualiffication Range for WPS per section IX

Hi Rafeeq,

WPS/PQR qualified for 8" dai. qualifies for 2 7/8" (73 mm) dia. and above.

sridhar

From: Karthik <karthik6684@yahoo.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Tuesday, 3 July 2012 2:25 PM
Subject: Re: [MW:14747] Diameter Qualiffication Range for WPS per section IX

Hi,
WPS can be qualified with either Pipe or Plate, and the qualified WPS can be used for both.
 
Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
German-Thai Boiler Engineering Cooperation Limited.
Rayong Factory ;
379 Moo.6 Soi 8, Tambol Pananikom,
Nikompattana, Rayong 21180 THAILAND
Tel : +66 38 897 035-9 Ext. 137
Fax : +66 38 897 034
Hand Phone: 0066 892512282


From: rafeeqmahadighar rahman <rafeeqmahadighar@yahoo.co.in>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Monday, July 2, 2012 11:31 PM
Subject: [MW:14742] Diameter Qualiffication Range for WPS per section IX

Dear Experts,
 
Accordance with section IX does the Pipe diameter range is an essential variable for WPS?
for example the PQR coupon has qualified on 8" dia, does it qualify for all or 2 7/8" and above.   
appreciate your valuable input.
 
Warm Regards'
Rafeeq
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.




No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...