Re: [MW:14592] USE of PQR of GTAW+SMAW for new WPS GTAW process only.

Dear Mr praveen,
                        Yes u can use it for the thickness range of 1.5to6mm with GTAW process and 2.5to10mm with SMAW process.


 
On Mon, Jun 11, 2012 at 9:32 AM, Parveen Kumar Nakwal <pknakwal@gmail.com> wrote:
Dear Experts,

Can we use S.S to S.S 8mm base metal thickness PQR of GTAW (3mm)+SMAW (5mm) for the making for new WPS of S.S to S.S with GTAW only, with 2mm base metal thickness only ? 

Waiting for reply..

Regards.
Parveen K. Nakwal

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
THANKS & REGARDS

KALYAN VVV
WELDING EXECUTIVE ENGINEER
HYDERABAD


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...