Hi all,Could you please interpret the code sub clause correctly.What does it actually meant by?the PWHT requirement is applicable only if it is above 25mm thick for NPS 12 or above diameter openings?5.7.4.2 When the shell material is Group I, II, III, or IIIA, all opening connections NPS 12 or larger in nominal diameter
in a shell plate or thickened insert plate more than 25 mm (1 in.) thick shall be prefabricated into the shell plate or
thickened insert plate, and the prefabricated assembly shall be thermally stress-relieved within a temperature range of
600°C – 650°C (1100°F – 1200°F) for 1 hour per 25 mm (1 in.) of thickness prior to installation. The stress-relieving requirements need not include the flange-to-neck welds or other nozzle-neck and manhole-neck attachments, provided
the following conditions are fulfilled:
a. The welds are outside the reinforcement (see 5.7.2.4).
b. The throat dimension of a fillet weld in a slip-on flange does not exceed 16 mm (5/8 in.), or the butt joint of a weldingneck
flange does not exceed 19 mm (3/4 in.). If the material is preheated to a minimum temperature of 90°C (200°F) during
welding, the weld limits of 16 mm (5/8 in.) and 19 mm (3/4 in.) may be increased to 32 mm and 40 mm (11/4 in. and 11/2 in.),
respectively.
Cheers,Thomas Cholamattam
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment