Dear Devarajan,
As para QW-423.1 of ASME Section IX  Base metal used for welder qualification may be substituted for the metal specified in the WPS in accordance with the following table. Table is mentioned as follow

Base Metals for Welder Qualification

Qualified Production Base Metals

P-No. 1 through P-No. 15F, P-No. 34, and P-No. 41 through P-No. 49

P-No. 1 through P-No. 15F, P-No. 34, and P-No. 41 through P-No. 49

  so we can substituted base metal without qualified any PQR is it the interpretation of this clause.

On Sat, Sep 10, 2011 at 7:49 AM, Devarajan Ramasamy <neo.devarajan@gmail.com> wrote:

Dear Vijay,
 
You never mentioned the welding process that you are going to use for the welding, but as per ASME Sect IX, all the available welding process has P. No as an essential variable, which means you cannot use P8 qualification record to qualify P1 WPS.
 
But, if you have a WPS of P8 - P8 and your intention is to qualify your welder for this WPS using P1 as your base material, you can do so by quoting
 
QW-423.1 Alternate Base Metal for Welder Qualification
- In essence, Welder Qualification using P1 base metal qualifies for P1 to P11 material as long as your filler wire/ electrode is equivalent as per your WPS.
Hope this answers your query.

 
On Sat, Sep 3, 2011 at 3:21 AM, vijay Katkar <katkar.vijay22@gmail.com> wrote:
Dear Kundan/Mayur,



ASME Section IX Welder Qualification related Question.



As mentioned in section IX for qualification of welder or welding
operator use qualified WPS with supporting PQR's, if our PQR is welded
with P No- 8 to P No-8 (SA 240 TP 316L TO SA 240 TP 316L).

Is it possible to make WPS with P No-1 to P no-1 (PQR is with P No -8
To P No-8)  but other than p no  all variable are same as used in PQR
(Like filler wire, shelding  gas, purging if require or etc), this WPS
will use only for welder qualification. please guide us.



Vijay Katkar

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
This message originated from the Internet. Its originator may or may not be who they claim to be and the information contained in the message and any attachments may or may not be accurate.

This email transmission is intended solely for the named recipient(s). It may contain confidential and/or privileged information.If you are not the intended recipient, note that disclosing, copying or distributing it may be unlawful. Please notify the sender immediately if you have received it by mistake, and delete it from your system.
Internet communications cannot be guaranteed to be timely, secure, error or virus-free. The sender does not accept liability for any errors or omissions.

"SAVE PAPER - THINK BEFORE YOU PRINT!"

Regards,

~ DEVARAJAN RAMASAMY~

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...