Dear Sir(@MPK),

 

The copy’s you send mentions requirements for spacing between longitudinal welds, Mr. Pradip is asking for spacing between butt welds in pipe so in my opinion he’s talking about circumferential welds!

 

Met vriendelijke groeten / Best Regards

 

Herman Pieper

 

Pieper Quality Support & Inspection

Phone: +31 (0)521 380083

Fax:     +31 (0)84 7539225

Cell:     +31 (0)6 51691215

www.pieper-qsi.nl

 

Van: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] Namens mpk mpk
Verzonden: zaterdag 10 september 2011 11:36
Aan: materials-welding@googlegroups.com
Onderwerp: Re: [MW:12407] Distance between two butt joints in pipe weld

 

Dear,

 

Please find attached copies.

 

Thank you

MPK

On Sat, Sep 10, 2011 at 2:50 AM, tong tong <tong2je@gmail.com> wrote:

B31.3 is silent about that..so you need to refer back to project or client specification..some of client specify 2x or 50mm..

 

On Fri, Sep 9, 2011 at 2:33 PM, iulian oprea <iu_oprea@yahoo.com> wrote:

 

Linde Engineering standards says:

 

5 time of thickness, or 50 mm, whichever is greater.

 

regards

Iulian Oprea

From: pradip kumar sil <pradipsil@gmail.com>
To: materials-welding@googlegroups.com
Sent: Friday, September 9, 2011 7:23 AM
Subject: [MW:12383] Distance between two butt joints in pipe weld

 

Dear exparts,

As per ASME B  31.3 what is the minium spacing to be maintened between two butt weld in pipe & where is it mentioned

Is it three times of thickness or 25 m.m  whichever is greater.

Regards

Pradip --
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...