Re: [MW:12404] Impact test requirement for JO and JR grades in structural fabrication.


Yes CVN is mandatory. you may carry out the impact test as per requirement and
if it passes go ahead


On Sat, 10 Sep 2011 13:59:21 +0530 wrote
>Dear Experts,

For crosshead installation in jetty project, the following materials (37mm) are
used.


Road way����������� - S355JO
Crosshead���������� - S355JR & S275JR
Pipe track����������� - S355JR

As per European structural steel standard EN10025 , for JR grade, Longitudinal
charpy V-notch impacts 27J @20 degrees and for JO grade, Longitudinal charpy V-
notch impacts 27J @ 0 degrees.


We received materials mill certificates w/o impact test.

My question is whether impact is mandatory for above grades or any criteria of
thickness as per EN10025? Please mention with reference codes.


Your valuable suggestions are appreciated.

Regards

arvinda




--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-
welding+unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-
welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions w.r.t.
applicable code/standard/contract documents.
>


Dear Sir,





Thanking You,

Honesty is the best Policy

With Warm Regards,

Muthu Barathi P
Mobile No:00962788269821 (Jordan)
00962775401951

Treat yourself at a restaurant, spa, resort and much more with Rediff Deal ho jaye!

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...