Re: [MW:9447] SAW filler for SA516 Gr70

F7A4 - EM12K it self sufficient. No need to go for High magnese EM 14K..
 

BR,
MSMS
On Sat, Jan 15, 2011 at 12:14 AM, rinshad abdul rahman <rinshad043@gmail.com> wrote:
Dear all,

Which is the suitable filler for SAW on SA 516 Gr70 (with PWHT) ?

EM12K or EM14K

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...