Re: [MW:9435] WELD OF ATTACHMENT

Dear sir,
the weld between of a pressure vessel with a support that must be qualified according ASME Sec IX.
please refer ASME section VIII div I (refer clients specification also.)


 -------------
Thanks & Regards.

Santosh Gaikwad

Material Testing & Inspection Services(MTIS),
Surat,India.



On Sun, Jan 23, 2011 at 3:26 PM, Ali Asghari <asghariali@rocketmail.com> wrote:
Dear All
the weld between of a pressure vessel with a support that must be qualified according AWS D1.1OR ASME VIII?
REGARDS

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



-

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...