Monday, January 24, 2011

RE: [MW:9422] RE: 9372] AC welding for P5A & P5C

Hi Bhavesh,

You must have noted the excellent in-depth clarification on this matter from my learned friend Mr. P Goswami, P Eng.

Forum is definitely enriched & benefitted due to such contributors .

Best Regards..Amitabha

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Bhavesh Patel
Sent: Saturday, January 22, 2011 9:56 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:9401] RE: 9372] AC welding for P5A & P5C

 

Thanks Amitabha,

 

As I know by AC welding oxygen pick up (Generally 160~200 ppm) during welding is quite less than DC welding (Generally 250~300 ppm) which gives you a better toughness property.

 

But, how the Oxygen pick up is less in AC welding?

 

Kindly explain mechanism of the same.

 

Regards,

Bhavesh Patel

 

On Fri, Jan 21, 2011 at 5:33 PM, amitabha.bhattacharya <amitabha.bhattacharya@bwgindia.com> wrote:

Hi Bhavesh,
You may expect higher toughness values with AC welding for CrMo-steels.
Thanks
Amitabha

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of JIGO
Sent: Friday, January 21, 2011 2:55 PM
To: Materials & Welding
Subject: [MW:9372] AC welding for P5A & P5C

Dear All,


Why we are using AC current for SAW welding in low alloy steel (Mainly
for P5A & P5C) ?

Kindly share your valuable input.


Regards,
Bhavesh Patel
ISGEC, Dahej

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...