Mr.Anand ,
 
As per stated like Mr.Elshan , It is not at all recommended practice .I do not know where you have get this practice .Particularly Stainless steels 4mm Thk  does not resist much heat input when you making double V welding .....
 
Regards
 
Suresh

On Fri, Jan 21, 2011 at 5:02 PM, deco0404 <declan1foley@eircom.net> wrote:
Are you talking about double-operating, where you have a welder on
each side of the weld working at the same time. Not very common, but
have seen it done on tanks.....

On Jan 21, 8:47 am, Pushpraj Anand <pushprajanan...@gmail.com> wrote:
> CAN ANY BODY TELL ME THE PROCEDURE OF MAKEING DOUBLE V ON 4 MM STAINLESS
> STEEL PLATE
>
> --
> Regards,
> Pushpraj Anand

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks  & Best Regards,

Suresh

Mobile No: 91-92 92 905 905

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...