Friday, January 21, 2011

Re: [MW:9382] Will fillet welder qualified to tack the groove Joint


Yes he can do for groove joint fit up (tack weld only) if he was qualified in fillet weld.

Regads
Bijaya
On Fri, 21 Jan 2011 17:36:33 , Shashank Vagal <nach_sam@yahoo.com> wrote
No

--- On Fri, 21/1/11, Moorthy K. Rama <krama_m@yahoo.com> wrote:

From: Moorthy K. Rama <krama_m@yahoo.com>
Subject: Re: [MW:9375] Will fillet welder qualified to tack the groove Joint
To: materials-welding@googlegroups.com
Date: Friday, 21 January, 2011, 4:25 PM

Please refer Babu's question
Will the ASME fillet welder (Qualified welder) ,qualified to tack weld the  groove joint in fitup ?

Regards
 


From: César Alexis Viteri Pérez <alexis_viteri@hotmail.com>
To: Material Welding <materials-welding@googlegroups.com>
Sent: Fri, January 21, 2011 2:20:23 PM
Subject: RE: [MW:9373] Will fillet welder qualified to tack the groove Joint

Hi,
 
Mr. Suresh is right, for B31.3 u have to do tacks with qualified welder, see para 3.28.5.1-c:

 

(c) Tack welds at the root of the joint shall be made

with filler metal equivalent to that used in the root pass.

Tack welds shall be made by a qualified welder or welding

operator. Tack welds shall be fused with the root

pass weld, except that those which have cracked shall

be removed. Bridge tacks (above the weld) shall be

removed.
 
Best Regards

 

Date: Fri, 21 Jan 2011 14:37:25 +0530
Subject: Re: [MW:9368] Will fillet welder qualified to tack the groove Joint
From: bobsuresh24@gmail.com
To: materials-welding@googlegroups.com

I think No ,
 
Tack weld shall be done by qualified welder .
 
Regards
 
Suresh

On Fri, Jan 21, 2011 at 1:45 PM, Kathalingam Babu <kathalingam.qaqc@ppl.com.sg" target=_new>kathalingam.qaqc@ppl.com.sg> wrote:
Hi all
 
Any one share official interpretation for the below situation.
 
Will the ASME fillet welder ,qualified to tack weld the  groove joint in fitup ?
 
Thanks & Regards,
 
K. Babu

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding%2Bunsubscribe@googlegroups.com" target=_new>materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks  & Best Regards,

Suresh

Mobile No: 91-92 92 905 905


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...