Friday, January 21, 2011

Re: [MW:9363] matetrial data sheet

http://www.steadfast.co.uk/barspec.htm
or

TYPICAL ANALYSIS



C.

Si.

Mn.

Cr.

Mo.

0.45%

0.25%

0.85%

1.10%

0.25%


 

     AISI 4145 30-36HRc Typical Mechanical Properties 

 

Yield
(psi)

UTS
(psi)

%
Elongation


Reduction of Area

Hardness
HRC



Charpy
room temperature
(average of 3)

min 110k

min 135k

min 14%

min 40%

30-36



54J



Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Fri, 1/21/11, Elshan Feyzullayev <elshan_f@hotmail.com> wrote:

From: Elshan Feyzullayev <elshan_f@hotmail.com>
Subject: [MW:9361] matetrial data sheet
To: materials-welding@googlegroups.com
Date: Friday, January 21, 2011, 1:21 PM

Dear friends,
 
can some one have the data sheet for AISI 4145 material? I need the mechanical properties most likely YS and TS values shown on the certificate or data sheet.
 
kind regards,
elshan.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate