Thursday, January 20, 2011

Re: [MW:9342] AWS Table 5.8 doubt???

Hi,
As per AWS-Section5-Fig.5.4 weld size means - Lug size.

Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Wed, 1/19/11, Srinivas Engr <srinivas.gmsrini@gmail.com> wrote:

From: Srinivas Engr <srinivas.gmsrini@gmail.com>
Subject: [MW:9333] AWS Table 5.8 doubt???
To: "Materials & Welding" <materials-welding@googlegroups.com>
Date: Wednesday, January 19, 2011, 10:50 PM

Dear all,

AS per AWS.I knw tat for fillet weld sizes we have to refer Table 5.8.
My doubt is they given as weld size.
weld size refer to throat or leg length? which one tat refers?
clear me

Thanks & Regards
Srinivas

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...