Dear JJ,
 
I would think , you need to see if all the requirements of SA 350LF2, Cl1 are being met or not. Getting dragged on to only one property may not be right. If all other properties are within the specification requirements , it may be worthwhile to seek an explanation from the mill/supplier.
 
Errors in test results could be due to many things.
 
Thanks.
 
Pradip Goswami,P.Eng.
Welding & Metallurgical Specialist & Consultant
Email-pgoswami@sympatico.ca,
 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Kathalingam Babu
Sent: Tuesday, January 18, 2011 11:09 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:9319] Higher value of UTS, acceptable?

Hi
 
Since spec. clearly indicates the range, it has be to within the range, otherwise not acceptable
 
Thanks & Regards,
 
K. Babu

----- Original Message -----
Sent: Wednesday, January 19, 2011 11:47 AM
Subject: [MW:9317] Higher value of UTS, acceptable?

Dear all,
 
I have a material A350 LF2, CL1  with UTS of 724MPa (As mentioned in TC of Manufacturer).
 
As per ASME Sec IIA, requirement is 485 - 655 Mpa.
 
The higher value of UTS beyond the spec requirements is aceptable?
 
Thanks.
Regards,
JJ

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...