hi,
refer QW423 for P.No.qualification.But while welder weld CS to SS or vice versa...
pls.take care about F.No.qualifications as per QW433 and QW350 for essential variables.

Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Tue, 1/18/11, krishna <wiqw@rediffmail.com> wrote:

From: krishna <wiqw@rediffmail.com>
Subject: [MW:9281] welder qualification from cs to ss and vice versa
To: "materialswelding" <materials-welding@googlegroups.com>
Date: Tuesday, January 18, 2011, 11:46 AM

dear all,
                     how a welder qualified in carbon steel can also weld stainless steel and vice versa?

my question is where in ASME sec ix it is given ?

pls clarify

regards,
kk

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...