Hi Saamy,

SA-106 is a Standard Specification for Carbon Steel Pipe for High-Temperature Service whereas SA-333 is a Standard Specification for Seamless and Welded Steel Pipe for Low Temperature Service, I don't see any reason to compare both the materials.

Regards
Manpreet Singh


On Sun, 16 Jan 2011 22:03:34 +0530 Saamy wrote
>Dear Experts!
> Could you explain how to determined these 2
>materials as High Temp CS and Low Temp CS, because of these materials
>chemical properties as well as same?
>
>Advance Thanks!
>
>
>Saamy
>
>--
>To post to this group, send email to materials-welding@googlegroups.com
>To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...