SDSS is better qualified rather than grouped to the ASME code - the welder should Also be G48 tested as the use is for corrosion purposes mostly.
The G48 of the welders SS test will fail!
A


From: materials-welding@googlegroups.com <materials-welding@googlegroups.com>
To: materials-welding@googlegroups.com <materials-welding@googlegroups.com>
Sent: Sun Jan 16 08:38:14 2011
Subject: [MW:9239] WQT for Duplex SS

Dear All,
 
 Welder is qualified in SS material,it required separately  to be qualified for Duplex SS material.
 
thanks and regards

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 ************************************************************************* This e-mail message and any attachments to it are intended only for the  named recipients and may contain confidential information. If you are not one of the intended recipients, please do not duplicate or forward this e-mail message and immediately delete it from your computer. If you  received this email in error, please notify postmaster@veoliawater.com *************************************************************************       

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...