hi,
do u have asme sec.IX/EN codes?..any how in your case...qualify to 20mm.if 13 and more is unlimited for welder

Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Wed, 1/12/11, ELAMARAN RAJAN <elams.rajan@gmail.com> wrote:

From: ELAMARAN RAJAN <elams.rajan@gmail.com>
Subject: [MW:9199] Reg wqt for saw
To: materials-welding@googlegroups.com
Date: Wednesday, January 12, 2011, 9:38 PM


Dear friends
greetings of the day
I want a clarification against the saw welder qualification
During Wqt Welder welded saw by 10mm thickness then what was the range of thickness qualification
any one have the wqt cerificate sample pls send to me
 
WITH REGARDS
 

--
maran

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...