Wednesday, January 12, 2011

Re: [MW:9193] Regarding GTAW Welding Machine

Dear Anand,
 
  You have to fallow as per your WPS&PQR what you have used for. and for GTAW welding machine there are number brands in indian market today.
 
 
Regards,
Ramu

On Wed, Jan 12, 2011 at 4:00 PM, Pushpraj Anand <pushprajanand34@gmail.com> wrote:
Dear All,
 
 
We are going to weld 4 mm / 6 mm stainless steel plate.Filler wire dia is 2.4 mm and tungsten electrode dia is 1.6 mm.
 
for welding machine what should be the output current range and maximum continuous current at 100% duty cycle. please suggest me which welding machine is best for this application .
 
we are manufacturing this product in india.

--
Regards,
Pushpraj Anand

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...